Say Goodbye to Ethyl Cellulose! A7011 Functional Resin — A New Low-Odor & High-Cleanliness Solution for Sinterable Conductive Pastes
Release time:2026-10-30
Background
With the iterative upgrading of the electronic paste industry, silver-coated copper pastes are gradually replacing conventional pure-silver systems. Meanwhile, sintering processes in the industry are undergoing innovation: sintering temperatures have dropped from over 800 °C to 400 °C-500 °C, and nitrogen-protected sintering is widely adopted. Conventional ethyl cellulose cannot be fully carbonized under such low-temperature and inert-atmosphere conditions, which tends to cause carbon residues, resulting in poor contact of conductive layers and appearance defects. Therefore, the industry is in urgent need of alternative resin carriers tailored for new-generation processes.
1. Application Scenarios
Applicable Products: Ceramic sinterable conductive pastes (silver-coated copper pastes, silver pastes and other systems)
Applicable Working Conditions: Preparation of conductive / decorative inks for ceramic electronic components requiring low-temperature sintering under nitrogen atmosphere, screen-printing application, and paste storage.
Core Demands & Pain Points
- Conventional ethyl cellulose cannot achieve complete carbonization under nitrogen atmosphere at 400-500 °C, and carbon residues impair electrical conductivity and surface appearance.
- Conventional systems generate strong odor, creating poor working conditions and heavy pressure on environmental compliance.
- Silver-coated copper / silver-powder pastes are prone to agglomeration, sedimentation and even gelation during storage, leading to scrappage, poor stability and inconsistent electrical performance.
- Screen clogging frequently occurs, resulting in poor screen-printing continuity and low yield.
- High sintering residues and sintering marks, insufficient carbonization cleanliness, which undermine substrate adhesion and conductive-layer performance.
2. Core Technical Solution
- Suitable Substrates: Glass, metal, ceramics (household appliance glass, ceramic electronic parts, etc.)
- Coating Resin System: A7011 ether-alcohol-solvent-based functional resin, solid content: 45 %, low acid value (< 1 mgKOH/g), specially developed for low-temperature sintering processes.
- Sintering Conditions: Complete sintering at a minimum of 350 °C; compatible with 400 °C-500 °C nitrogen-atmosphere sintering processes, delivering residue-free and mark-free performance.
- Key Performance Features:
- Storage Stability for Gold / Silver Powder & Silver-Coated Copper Powder: Excellent storage compatibility with metal powders. Effectively inhibits agglomeration and sedimentation of silver powder / silver-coated copper powder and extends paste service life.
- Adhesion: Good compatibility with glass and ceramic substrates. Residue-free and mark-free after sintering, providing stable adhesion foundation for conductive layers.
- Processability: Resists screen clogging and fits screen-printing processes. Low-odor formulation improves working environment and enhances production continuity.
- Carbonization Cleanliness: Fully decomposes under nitrogen atmosphere at 400 °C-500 °C. No residues or marks after calcination. Outstanding carbonization cleanliness without compromising electrical conductivity or appearance consistency of conductive layers.

3. Solution Comparison
Comparison Dimension | Conventional Ethyl Cellulose Solution | A7011 Functional Resin Solution | Core Advantages |
Sintering-Temperature & Atmosphere Compatibility | Requires air sintering above 700 °C; prone to residues under 400-500 °C nitrogen atmosphere | Minimum sintering at 400 °C; compatible with low-temperature nitrogen-atmosphere processes | Perfectly fits new-generation silver-coated-copper-paste processes and eliminates carbon-residue risks |
Adhesion | Carbon residues easily cause poor interlayer bonding | Residue-free and mark-free after sintering; compatible with glass / ceramic substrates | Ensures stable bonding between conductive layers and substrates and improves end-product reliability |
Storage Stability | Silver-coated copper / silver powder tends to agglomerate and settle; short paste service life | Good storage compatibility with metal powders; low agglomeration tendency | Reduces paste waste and lowers batch-defect rates |
Substrate Compatibility | Poor wetting performance on glass / ceramics in some systems | Excellent dispersion, wetting and encapsulation effects on inorganic pigments and substrates | Fits mainstream substrates such as household-appliance glass and ceramics for broader application coverage |
Application Experience | Strong odor, frequent screen clogging, poor working environment | Low odor, screen-clogging resistance, smooth screen-printing | Improves workshop environmental conditions and boosts production efficiency and yield |
Carbonization Cleanliness | Carbon residues readily form under low-temperature nitrogen atmosphere, harming conductivity and appearance | Fully decomposes above 400 °C under nitrogen atmosphere with high cleanliness | Stabilizes conductive-layer performance and enhances appearance consistency |
4. Conclusions & Selection Recommendations
Conclusion: A7011 functional resin serves as an ideal ethyl-cellulose replacement for low-temperature nitrogen-atmosphere sintering of silver-coated copper pastes. It integrates low odor, superior storage stability, easy processability and high sintering cleanliness. It effectively addresses carbon-residue pain points of conventional systems under 400-500 °C nitrogen sintering and meets production-and-application requirements for household-appliance-glass sintered tempering inks and ceramic conductive pastes.
Selection Recommendations:
- Recommended as an alternative resin carrier for sintered tempering inks for household-appliance glass, as well as ceramic sintered silver-coated-copper / silver pastes.
- Prioritize for mid-to-high-end scenarios with strict requirements for odor, sintering residues and storage stability.
- Adjust system viscosity with ether-alcohol solvents according to process requirements to adapt to diverse screen-printing conditions.

5. Professional Corporate Credentials
Our company focuses on R&D and application of functional resins and electronic-paste carrier materials. We possess mature supporting processes and practical application cases for household-appliance glass and ceramic electronic pastes. Especially for low-temperature nitrogen-atmosphere sintering of silver-coated copper pastes, we provide formula customization, free sample testing and bulk-supply services, complying with industrial environmental-protection standards and export requirements, and deliver end-to-end technical support for customers.
6. FAQ
Q1: Will A7011 really leave no carbon residues after sintering at 400 °C under nitrogen atmosphere?
A1: Yes. Specially engineered for low-temperature sintering, A7011 features a TGA decomposition range of 200 °C-450 °C. Complete decomposition is achieved at 400 °C. Even under nitrogen-protected sintering, calcination yields residue-free and mark-free surfaces with excellent carbonization cleanliness, without impairing conductivity or appearance consistency of conductive layers.
Q2: Will replacing ethyl cellulose with A7011 improve storage stability of silver-coated copper pastes?
A2: Yes. A7011 delivers outstanding encapsulation, dispersion and wetting performance toward metal powders including silver-coated copper powder and silver powder. It effectively suppresses powder agglomeration and sedimentation, greatly enhancing paste storage stability, extending service life and reducing batch-related defects.
Q3: Does A7011 produce strong odor during application? Does it cause screen clogging?
A3: A7011 adopts a low-odor ether-alcohol solvent system, with far weaker odor than conventional ethyl-cellulose systems, which greatly improves workshop working conditions. Besides, it resists screen clogging, fits standard screen-printing workflows and increases production continuity and finished-product yield.
For complete technical specifications, sample testing and customized formula proposals, please contact our account managers for one-on-one technical support and matching services.