Guangdong KDD Functional Materials Co., Ltd.
KDD MX2665 Flexible Modified Acrylic Resin | Solves Cracking, Deformation and Paint Peeling of Coatings on Soft TPU Substrates | Professional Low-Temperature High-Flexibility Coating Solution
Release time:2026-08-21
I. Application Scenarios
Applicable Products: TPU phone cases, TPU wearable device soft rubber accessories, TPU films, TPU hoses, shoe material TPU structural parts, smart band/watch soft rubber housings, 3C digital soft decorative parts, finish coats and protective clear coats for elastic plastic appearances.
Applicable Working Conditions: Automatic spraying, manual spraying, roller coating and flow coating processes; working conditions with repeated bending, stretching and extrusion deformation of soft substrates; scenarios with frequent manual touching, sweat and sebum contact, and slight alcohol wiping; mass production lines with low-temperature baking, production environments prone to deformation of thin-walled soft rubber parts, and internal and external sales 3C digital parts coating scenarios.
Core Demands and Pain Points:
1. Conventional acrylic resin films are hard with poor flexibility, leading to easy cracking, paint bursting and overall peeling of coatings on TPU substrates after bending and stretching, resulting in low product yield.
2. Ordinary coatings have weak interfacial adhesion with elastic TPU substrates, causing common defects such as surface peeling, delamination and edge warping during long-term service.
3. General commercial TPU coatings have poor resistance to hand sweat and human sebum, tending to become sticky, lose gloss and accumulate dust after long-term touching, which affects product appearance and service life.
4. Most resins require high curing temperatures, and high-temperature baking easily causes shrinkage, deformation and warpage of thin-walled TPU soft parts, failing to meet the mass production requirements of precision soft accessories.
5. General resins have narrow substrate adaptability, poor compatibility with TPU of different hardness and different processes (polyether/polyester type), resulting in cumbersome formula debugging and high inventory costs.

II. Core Technical Solution
1. Applicable Substrates: Full-range TPU substrates (polyester and polyether TPU), TPU injection-molded soft rubber parts, TPU films, modified TPU blended substrates, suitable for most 3C, shoe material and elastic plastic products.
2. Coating Resin System: KDD MX2665 flexible modified solvent-based acrylic resin. Adopting a special flexible molecular chain segment design, it can form molecular entanglement with elastic TPU substrates, featuring high adhesion, high elongation and film stability, and compatible with single-component air-drying and two-component PU crosslinking systems.
3. Curing and Baking Conditions: 60℃-80℃ × 15-20min (low-temperature baking to eliminate thermal deformation of TPU substrates); compatible with room-temperature air-drying processes.
4. Key Performance
It achieves extremely high elastic matching with TPU substrates, with no cracks, paint bursting or peeling after repeated bending and extrusion. The coating fully follows the dynamic deformation of substrates, completely solving the cracking problem of coatings on soft substrates.
Adhesion: It provides excellent wetting and penetration on smooth TPU soft substrates with strong interfacial bonding strength. It achieves Grade 0 in cross-cut test, with no adhesion attenuation, delamination or paint peeling after repeated deformation and damp-heat tests.
The film remains non-sticky and dust-free after long-term touching; it resists conventional alcohol wiping and slight daily chemical erosion, maintaining stable gloss and color fastness for long-term service.
III. Conclusion and Selection Recommendations
Conclusion: MX2665 is a customized flexible modified acrylic resin for soft elastic TPU substrates. It specifically solves the industry pain points of traditional coatings such as cracking and peeling, substrate thermal deformation, sweat-induced stickiness and narrow substrate compatibility. With the core advantages of low-temperature curing, ultra-high flexibility, strong adhesion and long-term stain and sweat resistance, it is perfectly suitable for the coating of TPU products including 3C digital products, wearable devices, shoe materials and elastic films, with stable performance that meets mass production standards and domestic and foreign sales quality requirements.
Selection Recommendations:
1. Prioritize MX2665 as the main finish resin for TPU phone cases and soft wearable accessories with frequent bending and touching.
2. Adopt the 60℃ low-temperature baking process for mass production of precision soft rubber parts to reduce defect rates and avoid substrate thermal deformation.
3. For working conditions requiring high weather resistance and wear resistance, formulate a two-component system with isocyanate curing agent to further improve chemical resistance and wear resistance.
4. For low-surface-energy TPU substrates, conduct oil removal and cleaning in advance or use supporting primer to improve mass production stability.

IV. Enterprise Professional Endorsement
KDD focuses on the R&D and application of functional modified acrylic resins and special coating resins for plastics. With years of in-depth experience in soft plastic and 3C digital coating materials, we have mature processes and mass production cases. We provide customized formula development, free sample testing, on-site process guidance and bulk supply services. All products comply with industry standards and EU RoHS and REACH export requirements.
V. FAQ
1. Q: Can MX2665 be directly sprayed on TPU substrates without primer?
A: It can be directly sprayed on clean conventional TPU substrates. For low-surface-energy and hard-to-adhere modified TPU, matching with special primer can further improve adhesion and bending resistance reliability to achieve zero peeling defects in mass production.
2. Q: Can the baking temperature be increased? Will high temperature damage TPU workpieces?
A: The recommended optimal process is 60℃-80℃ × 15-20min. Temperatures above 70℃ may cause shrinkage and deformation of thin-walled TPU parts, so high-temperature baking is not recommended. Extending flash-off time can optimize film performance.
3. Q: How is the sweat resistance and anti-sticking performance of MX2665 cured film?
A: Modified for sweat and sebum resistance, the film resists stickiness, dust accumulation and gloss loss during long-term frequent touching. It is fully applicable to terminal consumer products such as phone cases and watch bands with excellent long-term appearance durability.