KDD A7190 | Water‑Soluble Acrylic Resin for Tobacco Inner Liner Gravure Ink — High‑Speed Printing, Low‑VOC, Solves Blocking & Ink‑Falling Issues
Release time:2026-08-27
1. Application Scenarios
Applicable Products: Water-based color inks for gravure printing of cigarette outer inner liner paper, cigarette package liner paper and tipping inner liner paper (solid color inks including red, yellow, blue, black, etc.)
Applicable Working Conditions: Rotary gravure high-speed printing (80‑180m/min), water-alcohol dilution system; the printed materials are rolled up and stacked for subsequent die-cutting, folding and packaging; compliant with tobacco packaging environmental control requirements for low odor and low solvent residue.
Core Industry Pain Points
1. Ordinary water-soluble resins have poor redissolvability, easily causing screen blocking and blade lines during high-speed gravure printing, resulting in incomplete dot transfer in fine screens and water ripple & mottling defects on solid color blocks.
2. The ink layer is brittle during folding and die-cutting of inner liner paper, leading to ink peeling and base exposure at creases and low finished product yield.
3. Inner liner paper is prone to moisture contact and ambient humidity fluctuation. Ordinary water-based inks have insufficient water resistance, causing ink whitening, smudging and color bleeding after moisture absorption.
4. Poor pigment dispersion leads to insufficient tinting strength of color inks, requiring a large amount of co-solvents in the formula, which results in high VOC, strong odor and failure to meet tobacco packaging safety control standards.
5. Narrow drying window: high oven temperature easily causes paper curling and wrinkling; low temperature leads to surface drying without core drying, resulting in back sticking of rolled prints and product adhesion.
2. Core Technical Solution
1. Applicable Substrates: Cigarette package base inner paper, aluminum-plated inner liner paper, special tobacco liner paper and thin tipping paper
2. Coating Resin System: KDD A7190 aminated water-soluble acrylic resin with excellent water-alcohol miscibility, superior pigment wettability and dispersibility, outstanding redissolvability, low odor and low VOC; compatible with water-based wax emulsions and various water-based additives.
3. Recommended Curing & Baking Conditions: 75℃ × 25s
- Firm ink layer that withstands die-cutting and creasing post-processing;
- Excellent adhesion: no ink peeling after tape peeling test on inner liner paper, stable adhesion in high-humidity environments, and anti-smudging performance during assembly line packaging.

3. Performance Comparison Between New and Traditional Solutions
Comparison Item | Traditional Resin Solution | KDD A7190 Solution | Core Advantages |
Drying Process | 85‑95℃ oven temperature; high temperature tends to cause curling and deformation of thin inner liner paper | Instant drying at medium-low temperature of 75℃, reducing paper thermal deformation risk, adapting to high-speed rotary production lines and lowering energy consumption |
Flexibility & Processability | Brittle ink layer, easy ink peeling and base exposure at folding creases | Balanced hardness and toughness molecular design with folding and die-cutting resistance, no ink peeling during post die-cutting & folding, reducing scrap rate and improving finished product qualification rate |
Moisture & Wipe Resistance | Prone to whitening under moisture and ink peeling after alcohol wiping | Stable ink layer with excellent moisture resistance and alcohol wipe resistance, eliminating smudging and color bleeding of tobacco packages during storage and ensuring stable finished product appearance |
Printing Adaptability | Poor wettability on thin inner paper, poor fine screen transfer, frequent screen blocking and blade lines | Universal compatibility with inner liner paper and aluminum-plated liner paper, excellent redissolvability and anti-blocking performance, complete dot restoration, smooth solid printing surface, fewer screen cleaning shutdowns and higher printing efficiency |
4. Selection Conclusion & Formula Recommendations
Conclusion
KDD A7190 water-soluble acrylic resin is specially developed for water-based color inks for gravure printing of cigarette inner liner paper. The water-alcohol compatible system featuresexcellent pigment dispersion and outstanding redissolvability, solving high-speed gravure printing problems including screen blocking, blade lines and incomplete fine screen transfer. It also delivers excellent ink layer flexibility, folding resistance, moisture resistance and wipe resistance. With medium-low temperature drying to prevent paper curling, low odor and low VOC compliance with tobacco packaging environmental and safety standards, it eliminates full-process pain points in printing, post-processing and storage.
Selection Recommendations
1. Prioritize A7190 for water-based solid color inks used in gravure printing of cigarette outer inner liner paper and tipping inner liner paper.
2. Recommended for high-speed rotary gravure production lines with frequent problems of screen blocking, blade lines, folding ink peeling and roll-back sticking.
3. Formula Suggestion: Water + a small amount of ethanol co-solvent system, pH value controlled at 7.5‑8.5; adding water-based wax emulsion can further improve wear resistance and anti-sticking performance.
KDD focuses on the R&D and supply of water-based and alcohol-soluble acrylic resins for tobacco packaging. We have mature application cases and provide customized formula services, sample testing and bulk supply to meet industry and export standards.

5. FAQ
Q1: What is the optimal pH range for water-based color inks made with A7190 for inner liner paper?
A: The pH value of finished ink is recommended to be controlled at 7.5‑8.5. Too low pH will weaken the water solubility of the resin; too high pH will increase odor and damage water resistance performance.
Q2: How to adjust the formula and process to solve roll-back sticking during printing?
A: ① Ensure sufficient oven air volume for thorough drying; ② Add an appropriate amount of water-based wear-resistant wax emulsion to the formula; ③ Control the humidity of the printing workshop to reduce residual moisture, which can significantly improve back sticking.
Q3: Can A7190 be blended with emulsions?
A: It can be blended with compatible acrylic emulsions to further optimize the water resistance and wear resistance of the ink layer. Small-scale compatibility tests are required first to confirm no precipitation or delamination before mass production.